Cold stamping die welding hardness less than the phenomenon: 

The reason :( a) 

When the welding current is too large, the mold base material dilution ratio is too large, damage to the die base metal alloy elements. 

Responses: 

Try using a small current, short-arc welding, welding rod swing amplitude is not greater than 1.5 times the diameter of the electrode. 

The reason :( two) 

And the layer between the preheating temperature during welding temperature is not controlled. 

Responses: 

Pay attention to grasp preheat temperature (preheating temperature and carbon content of the base material is mainly concerned), and a control layer temperature during welding. 

The reason :( three) 

Surfacing layers excessive, improper selection of welding materials. 

Responses: 

Selection of welding materials for cladding layers required. (Some of the welding material of high hardness is directly organizer martensite, and some welding surfacing material is a three or more when it can be transformed from austenite to martensite of the high hardness.)


Send Inquiry